  1. In 1939 Heirich Stockler of Leitz came out with a developer which gave highest possible sharpness without loss of speed

     

    Solution A

     

    metol 5 gram

    sodium sulphite 100 gram

    in 1000 cc water

     

    Solution B

     

    borax 10 gram

    in 1000 cc water

     

     

     

    develop film in solution A for 2-5 minutes 68 degree F

     

    follow by development in solution B for 3 minutes

     

    Do not rinse film between baths

     

    Source Aaron Sussman The Amateur Photographer's Handbook

  2. The 110 format film available now is color only, which I cannot develop my self. I want to shoot B&W 110 film which I can develop at home.

    So the only way is to use a film slitter to cut ASA 100 35mm film into

    16mm wide film strips, and reload into an empty 110 cassette

  3. I try to reload 16mm bulk film into 110 cassette for my Pentax auto 110 film camera.

     

    The currently available 16mm bulk film are low speed type (ASA 25), cannot be use

     

    in pentax 110, which need at least ASA 100.

     

    In a 1950 book published 1952 in Singapore there is a quote from American Photography

    1939 March edition a formula which can increase film speed from ASA 8 to ASA 450, a film speed boost to 40x.

     

    However one of his ingrediant Johnson & Johnson Swerl was discontinued long time ago

     

    Any one knows any film speed booster developer, when can boost ASA 25 TO ASA 100

×
×