  1. <p>Hello,</p> <p>Hope that someone can help me with this as I am going out of my mind! :)<br /> The first time I tried the Caffenol C-M recipe (http://caffenol.blogspot.com/2010/03/caffenol-c-m-recipe.html) it worked like a charm. I got two beautifully developed films.</p> <p>Now the second and third time the films came out almost completely transparent. You can see a glimpse of what was photographed and the overexposed parts (black parts on film) are very soft on the touch, almost like gelatine and can be peeled away very easily. There were two films in the last tank I developed: The first one (Rollei Retro) came out fine, while the other (Ilford HP5 Plus) has the aforementioned problems.</p> <p>Attaching two images of the film.</p> <p>Does anyone have an idea of why this is happening? I appreciate your response.</p> <p>Attaching two images <br> Regards,<br /> Mario</p><div></div>
×
×